A Study on Multi-defect Constrained Bendability of Thin-walled Tube NC Bending Under Different Clearance

查看全文 作  者:LI Heng YANG [1]He 高影响力作者 机构地区:[1]State Key Laboratory of Solidification Processing, School of Materials Science and Engineering~ Northwestern Polytechnical University, Xi'an 710072, China高影响力机构 出  处:《Chinese Journal of Aeronautics》索引2011年第24卷第1期,共11页高影响力期刊 基  金:National Natural Science Foundation of China (59975076, 50905144);State Key Laboratory of Materials Processing and Die & Mould Technology, Huazhong University of Science and Technology (09-10);NPU Foundation for Fundamental Research (JC201028);Fund of the State Key Laboratory of Solidification Process-ing in NWPU 摘  要:Thin-walled tube numerical control (NC) bending is a tri-nonlinear physical process with multi-defect and multi-die constraints. The clearance on each contact interface is the major factor to indicate the contact conditions. A three-dimensional-finite element (3D-FE) model is established to consider the realistic dynamic boundary conditions of multiple dies under ABAQUS/Explicit platform. Combined with experiment, numerical study on bending behavior and bendability under different clearance between tube and various dies is conducted in terms of wrinkling, wall thinning and cross section deformation. The results show that (1)with smaller clearance of tube-wiper die and tube-mandrel, the wrinkling can be restrained while the wall thinning It and cross-section deformation Id increase; while excessive small clearance blocks tube materials to flow past tangent point and causes piles up, the onset of wrinkling enhances It and Id. (2)Both It and Id decrease with smaller clearance of tube-pressure die; the wrinkling possibility rises with larger clearance on this interface if the mandrel’s freedom along Y-axis is opened; smaller clearance of tube-bend die prevents wrinkling while increases It, and the clearance on this interface has little effect on Id. (3)A modified Yoshida buckling test (YBT) is used to address the wrinkling mechanisms under normal constraints in tube bending: the smaller clearance may restrain wrinkling efficiently; the smaller wall thickness, the less critical clearance needed; the critical clearance for tube bending 38 mm×1 mm×57 mm (tube outer diameter×wall thickness×centerline bending radius) equals about 20% of initial wall thickness. 关 键 词:数控弯曲 弯曲性能 小间隙 薄壁管 缺陷 多约束 壁厚减薄 三维有限元
相关文献

参考文献(18)

引证文献(26)

耦合文献(34)

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费