Improved creep aging response in Al-Cu alloy by applying pre-aging before pre-straining

查看全文 作  者:Fangpu [1,2]LYU;Chunhui [1,2]LIU;Peipei [3]MA;Jianshi [2]YANG;Longhui [2]CHEN;Lihua [1,2]ZHAN;Minghui [1,2]HUANG 高影响力作者 机构地区:[1]State Key Laboratory of Precision Manufacturing for Extreme Service Performance,School of Mechanical and Electrical Engineering,Central South University,Changsha 410083,China;[2]Light Alloy Research Institute,Central South University,Changsha 410083,China;[3]Advanced Research Center,Central South University,Changsha 410083,China高影响力机构 出  处:《Chinese Journal of Aeronautics》索引2023年第36卷第7期,共13页高影响力期刊 基  金:support from the National Natural Science Foundation of China(Nos.52274404,U2032117,U22A20190);Natural Science Foundation of Hunan Province,China(No.2022JJ20065);the Science and Technology Innovation Program of Hunan Province,China(No.2022RC1001);the National Key Research and Development Program of China(No.2021YFB3400903). 摘  要:The improvement of post-form properties without compromising creep formability has been a critical issue in creep age forming of aluminum alloy component. A pretreatment process incorporating artificial pre-aging at 165 °C for 6 h/12 h/24 h followed by pre-strain(3%–9%)has been developed. This method not only evidently improves the strength but also accelerates the creep deformation during creep aging of an Al-Cu alloy. A strength increase of 50 MPa with a slight decrease of ductility relative to the 9% pre-strained alloy is acquired in the alloy artificially pre-aged for 24 h regardless of the pre-strain level(3%–9%). Artificial aging for 24 h prior to 3%pre-strain enables an increase of creep strain by 30%. The creep strain in the alloy artificially preaged for 24 h and pre-strained by 6% is comparable to that in the alloy pre-strained by 9%. The strength and ductility in the alloy artificially pre-aged for 6 h/12 h and pre-strained by 3% are even slightly higher than those in the alloy purely pre-strained by 9%. The characterizations by transmission electron microscopy reveal that pre-aging at 165 °C could promote the accumulation of dislocations during pre-straining due to the pinning effect of pre-existing Guinier-Preston zones(GP zones)/θ’’phases and thus expedite the creep deformation in respect to the pure pre-straining treatment. The enhanced precipitation of θ’phases at these pinned dislocations contributes to the improved strength after creep aging. The results demonstrate applying artificial pre-aging before pre-straining is an efficient strategy to elevate the creep aging response in Al alloys. 关 键 词:Al-Cu alloy Creep aging PRE-AGING PRECIPITATION PRE-STRAIN
相关文献

参考文献(42)

引证文献(1)

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费